The synthesis processes for ultradiamond50 and ultradiamond90 particles are briefly outlined. Outlines include starting materials, conditions of reaction (temperature, pressure, and time), and patent citations. Starting materials for ultradiamond90 include ultradiamond50. link to home link to index of topics link to glossary
link to products link to applications link to properties synthesis link to publications link to home


  Synthesis of ultradiamond50

Materials
Explosive-containing carbon, with a negative oxygen balance
Gases inert to carbon, containing 0.1 - 6.0 % oxygen by volume
Ultradispersed carbon condensate, 0.01 - 0.15 kilograms per cubic meter

Conditions of reaction
Temperature: 3,500 K (3227 deg. C)
Pressure: over 20 GPa (2,900,000 psi)
Time: 0.1 - 0.5 microseconds

For more information
US Patent 5,861,349



  Synthesis of ultradiamond90

Materials
ultradiamond50
An oxidizing mixture of sulphuric and nitric acids

Conditions of reaction
Temperature: 503 - 578 K (230-305 deg. C)

For more information
Russian Federation Patent 2041165


Advanced Materials for the 21st Century

| Search | Index | Glossary |
| Products | Applications | Properties | Synthesis | Publications | Home | Contact Us |

Copyright Ultradiamond Technologies Inc.Copyright, trademark and other legal notices